Medical and Dental Consultantsí Association of Nigeria
Home - About us - Editorial board - Search - Ahead of print - Current issue - Archives - Submit article - Instructions - Subscribe - Advertise - Contacts - Login 
  Users Online: 1117   Home Print this page Email this page Small font sizeDefault font sizeIncrease font size
 
ORIGINAL ARTICLE
Year : 2019  |  Volume : 22  |  Issue : 12  |  Page : 1758-1764

Do ozonated water and boric acid affect the bond strength to dentin in different adhesive systems?


1 Department of Restorative Dentistry, Faculty of Dentistry, Cumhuriyet University, Sivas, Turkey
2 Department of Restorative Dentistry, Faculty of Dentistry, Sakarya Univercity, Sakarya, Turkey

Correspondence Address:
Dr. E Akturk
Department of Restorative Dentistry, Faculty of Dentistry, Cumhuriyet University, Sivas - 58140
Turkey
Login to access the Email id

Source of Support: None, Conflict of Interest: None


DOI: 10.4103/njcp.njcp_281_19

Rights and Permissions

Aim: The aim of this in vitro study was to compare the effects of the application of three different cavity disinfecting agents to dentin on the micro-shear bond strength (μ-SBS) of one self-etch and two universal adhesive systems. Materials and Methods: In total, 120 caries-free human permanent molar teeth were used in this study. Mid-coronal dentin surfaces were revealed by cutting occlusal enamel and a standard smear layer was obtained by using 600-800-1200 grid silicon carbide abrasive papers. Specimens were randomly assigned to four groups according to the disinfectant used: Group 1: Control (no disinfectant); Group 2: 2% chlorhexidine based (Consepsis); Group 3: 10 ppm ozonated water (TeknO3zone); Group 4: 5% boric acid (Handmade). Each group was divided into three subgroups according to the type of adhesive (Clearfil SE Bond, OptiBond XTR, and Tokuyama Universal). Specimens were bonded using either Clearfil SE Bond, OptiBond XTR or Tokuyama Universal, which were employed according to the manufacturer's instructions. Resin composite microcylinders were bonded using Tygon® tubes for μ-SBS testing. After specimens were stored for 24 h, at 37°C in distilled water, μ-SBS test was measured with a universal test machine (LF Plus, Lloyd, Instrument). μ-SBS results were analyzed by one-way analysis of variance (ANOVA) and Tukey's tests. Results: When the mean microshear bond strength values of the control group were compared, the difference between the subgroups was not significant (P < 0.05). When the mean microshear bond strength values of the chx, ozonated water, and boric acid were compared, the difference between Clearfil SE Bond and Tokuyama Universal was significant (P < 0.05) and the difference between the other groups was not significant (P > 0.05). Conclusion: Ozonated water and boric acid may be as an alternative to other materials used as cavity disinfectants.


[FULL TEXT] [PDF]*
Print this article     Email this article
 Next article
 Previous article
 Table of Contents

 Similar in PUBMED
   Search Pubmed for
   Search in Google Scholar for
 Related articles
 Citation Manager
 Access Statistics
 Reader Comments
 Email Alert *
 Add to My List *
 * Requires registration (Free)
 

 Article Access Statistics
    Viewed79    
    Printed0    
    Emailed0    
    PDF Downloaded39    
    Comments [Add]    

Recommend this journal