Effect of saliva decontamination procedures on shear bond strength of a one-step adhesive system


1 Department of Restorative Dentistry, Faculty of Dentistry, Selcuk University, Konya, Turkey
2 Department of Pedodontics, Faculty of Dentistry, Selcuk University, Konya, Turkey

Correspondence Address:
Aİ Erkan,
Department of Restorative Dentistry, Faculty of Dentistry, Selcuk University, Selcuklu 42075, Konya
Turkey
Login to access the Email id

Source of Support: None, Conflict of Interest: None

Aim: To evaluate the effect of different saliva decontamination procedures on the shear bond strength of a one-step universal adhesive system (Single Bond™ Universal Adhesive, 3M ESPE, St. Paul, MN, USA). Materials and Methods: The occlusal surfaces of 75 human third molars were ground to expose dentin. The teeth were divided into the following groups: Group 1 (control group): Single Bond™ Universal Adhesive was applied to the prepared tooth according to the manufacturer's recommendations and light cured; no contamination procedure was performed. Group 2: Bonding, light curing, saliva contamination, and dry. Group 3: Bonding, light curing, saliva contamination, rinse, and dry. Group 4: After the procedure performed in Group 2, reapplication of bonding. Group 5: After the procedure performed in Group 3, reapplication of bonding. Then, composite resins were applied with cylindrical-shaped plastic matrixes and light cured. For shear bond testing, a notch-shaped force transducer apparatus was applied to each specimen at the interface between the tooth and composite until failure occurred. The data were statistically analyzed using one-way ANOVA. Results: One-way ANOVA revealed significant differences in shear bond strength between the control group and experimental Groups 2 and 4 (P < 0.05). No significant difference was found for experimental Groups 3 and 5 when compared to the control group (P > 0.05). Conclusion: The present in vitro study showed that water rinsing is necessary if cured adhesive resin is contaminated with saliva to ensure adequate bond strength.


Print this article
Search
 Back
 
  Search Pubmed for
 
    -  Ülker E
    -  Bilgin S
    -  Kahvecioğlu F
    -  Erkan A
 Citation Manager
 Article Access Statistics
 Reader Comments
 * Requires registration (Free)
 

 Article Access Statistics
    Viewed866    
    PDF Downloaded31    

Recommend this journal